| Komposisi Kimia | |||||||
| Nilai | Ni% | Cu% | Fe% | M N% | C% | Si% | S% |
| Menit 63 | 28-34 | Maksimal 2,5 | Maks 2.0 | Maksimal 0,30 | Maksimal 0,50 | Maksimal 0,024 | |
| Merek Internasional Monel 400 | ||||
| Amerika Serikat | GE | UK | FR | |
| UNS | JAHIT VDIUV | BS | AFNOR | |
| Monel 400 | Nomor telepon N04400 | Nomor W.2.4360 NiCu30Fe | NA 12 | Nomor 30 |
| Sifat Fisik | ||
| Nilai | Kepadatan | Titik lebur |
| Monel 400 | 8,83 gram/cm3 | 1300ºC-1390ºC |
| Sifat Mekanik | ||||
| Paduan | Kekuatan Tarik (Rm N/mm2) | Kekuatan hasil (RP0,2N/mm2) | Perpanjangan (A5%) | HB |
| Monel 400 | 480 | 170 | 35 | ≥331 |
| Standar Produksi | |||||
| Batang | Penempaan | Pipa | Lembaran/Strip | Kawat Las | |
| Standar | ASTM B164 | ASTM B564 | ASTM B165 | ASTM B127 | ERNiCu-7 |
Kawat Semprot Termal Lainnya
| Barang | Kandungan kimia | Zn | Cd | Pb | Fe | Cu | Saldo Total |
| seng murni | Nilai nominal | ≥99.995 | ≤0,002 | ≤0,003 | ≤0,002 | ≤0,001 | 0,005 |
| Barang | Inconel 625 | Ni95Al5 | 45CT | Monel 400 | Monel 500 | HC-276 | Cr20Ni80 |
| C | ≤0,05 | ≤0,02 | 0,01-0,1 | ≤0,04 | ≤0,25 | ≤0,02 | ≤0,08 |
| Mn | ≤0,4 | ≤0,2 | ≤0,2 | 2,5-3,5 | ≤1,5 | ≤1,0 | ≤0,06 |
| Fe | ≤1,0 | T/A | ≤0,5 | ≤1,0 | ≤1,0 | 4.0-7.0 | T/A |
| P | ≤0,01 | ≤0,01 | ≤0,01 | ≤0,01 | ≤0,01 | ≤0,01 | ≤0,02 |
| S | ≤0,01 | ≤0,01 | ≤0,01 | ≤0,01 | ≤0,01 | ≤0,01 | ≤0,01 |
| Si | ≤0,15 | ≤0,2 | ≤0,2 | ≤0,15 | ≤0,5 | ≤0,08 | 0,75-1,6 |
| Cu | T/A | T/A | T/A | istirahat | 27-33 | T/A | T/A |
| Ni | istirahat | istirahat | istirahat | 65-67 | istirahat | istirahat | istirahat |
| Co | T/A | T/A | T/A | T/A | T/A | T/A | T/A |
| Al | ≤0,4 | 4-5 | T/A | ≤0,5 | 2.3-3.15 | T/A | T/A |
| Ti | ≤0,4 | 0,4-1 | 0,3-1 | 2.0-3 | 0,35-0,85 | T/A | T/A |
| Cr | 21.5-23 | ≤0,2 | 42-46 | T/A | T/A | 14.5-16 | 20-23 |
| Nb | 3.5-4.15 | T/A | T/A | T/A | T/A | T/A | ≤1,0 |
| Mo | 8.5-10 | T/A | T/A | T/A | T/A | 15-17 | T/A |
| V | T/A | T/A | T/A | T/A | T/A | ≤0,35 | T/A |
| W | T/A | T/A | T/A | T/A | T/A | 3.0-4.5 | T/A |
| Kotoran | ≤0,5 | ≤0,5 | ≤0,5 | ≤0,5 | ≤0,5 | ≤0,5 | ≤0,5 |
3. C276kawat semprot termal
Nama Umum: Oxford Alloy® C-276 FM C-276 Techalloy 276
Standar: AWS A5.14, ERNiCrMo-4/ ASME II, SFA-5.14, UNS N10276 Werkstoff Nr. 2.4886 ISO SNi6276 Eropa NiCrMo16Fe6W4
KOMPOSISI KIMIA (%)
| C | Si | Mn | S | P | Ni | Co |
| ≤0,02 | ≤0,08 | ≤1,0 | ≤0,03 | ≤0,04 | Istirahat | ≤2,5 |
| W | V | Fe | Cu | Cr | Mo | yang lain |
| 3.0-4.5 | ≤0,35 | 4.0-7.0 | ≤0,5 | 14,5-16,5 | 15-17 | <0,5 |